MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® CR-6100 Carbon-Reinforced Fluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: DuPont™ Vespel® CR-6100 is a composite material designed for use in hostile chemical environments. Stationary parts in this composite material meet the following specification per API STD 610/ISO 13709, Centrifugal Pumps For Petroleum Petrochemical and Natural Gas Industries:-46 to 230 °C (-50 to 450 °F) temperature limits and 2,000 kPa (20 bar; 300 psi) limiting pressure differential per wear part linear measure of 25 mm (1.0 inch). Due to its low creep and high thermal resistance, Vespel® CR-6100 often excels where other chemically-resistant plastics fall short. This makes Vespel® CR-6100 particularly well suited for seals, wear rings and other components used in a variety of devices and operating conditions. In addition, Vespel® CR-6100 material has been approved for use in potable water applications in the United Kingdom and Australia per the "Water Regulations Advisory Scheme (WRAS) Tests on Water Quality" based on the methods described in British Standards Institution, BS6920.

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.06 g/ccASTM D792
Water Absorption 0.010 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82x-y; ASTM D2240
 84z; ASTM D2240
Tensile Strength 2.80 MPa
@Temperature 260 °C
z; ASTM D3039
 17.0 MPa
@Temperature 22.8 °C
z; ASTM D3039
 52.0 MPa
@Temperature 260 °C
x-y; ASTM D3039
 120 MPa
@Temperature 22.8 °C
x-y; ASTM D3039
Elongation at Break 0.40 %
@Temperature 22.8 °C
z; ASTM D3039
 1.2 %
@Temperature 260 °C
x-y; ASTM D3039
 1.3 %
@Temperature 22.8 °C
x-y; ASTM D3039
 1.6 %
@Temperature 260 °C
z; ASTM D3039
Tensile Modulus 330 MPa
@Temperature 260 °C
z; ASTM D3039
 2680 MPa
@Temperature 22.8 °C
z; ASTM D3039
 2800 MPa
@Temperature 260 °C
x-y; ASTM D3039
 9790 MPa
@Temperature 22.8 °C
x-y; ASTM D3039
Flexural Strength 43.0 MPa
@Temperature 260 °C
x-y; ASTM D790
 156 MPa
@Temperature 22.8 °C
x-y; ASTM D790
Flexural Modulus 3720 MPa
@Temperature 260 °C
x-y; ASTM D790
 9530 MPa
@Temperature 22.8 °C
x-y; ASTM D790
Compressive Strength 18.0 MPa
@Temperature 260 °C
x-y; ASTM D695
 84.0 MPa
@Temperature 260 °C
z; ASTM D695
 87.0 MPa
@Temperature 22.8 °C
x-y; ASTM D695
 174 MPa
@Temperature 22.8 °C
z; ASTM D695
Compressive Modulus 720 MPa
@Temperature 260 °C
z; ASTM D695
 1730 MPa
@Temperature 260 °C
x-y; ASTM D695
 2070 MPa
@Temperature 22.8 °C
z; ASTM D695
 8520 MPa
@Temperature 22.8 °C
x-y; ASTM D695
Shear Strength 17.0 MPax-y Interlaminar; Internal Test
Izod Impact, Notched 2.00 ft-lb/inz; ASTM D256
 3.00 ft-lb/inx-y; ASTM D256
Izod Impact, Unnotched 3.00 ft-lb/inz; ASTM D256
 5.00 ft-lb/inx-y; ASTM D256
Limiting Pressure Velocity 9.70 MPa-m/sec
@Pressure 1.72 MPa
x-y; Falex Test
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.60 µm/m-°C
@Temperature 23.0 - 260 °C
x-y; ASTM E831
 300 µm/m-°C
@Temperature 35.0 - 149 °C
z; ASTM E831
 470 µm/m-°C
@Temperature 149 - 204 °C
z; ASTM E831
 750 µm/m-°C
@Temperature 204 - 260 °C
z; ASTM E831
Thermal Conductivity 0.700 W/m-K
@Temperature 23.0 - 149 °C
Hot Wire Method
Deflection Temperature at 1.8 MPa (264 psi) 120 °Cz; ASTM D648
 315 °Cx-y; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® CR-6110 Carbon-Reinforced Fluoropolymer
LKAB Minerals FordaGard Aluminum Hydroxide
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
Potters Industries Q-Cel® 5023
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting

PDTA7747a / 183708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.