MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wieland Porta P6 PFM Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Platinum Alloy

Material Notes: Gold-platinum-palladium ceramic alloy

Applications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneering

Dental

Key Words: EN ISO 9693
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 18.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 220HV5/30; after porcelain firing
 230HV5/30; hardened
Tensile Strength, Yield 82670 psi
@Strain 0.2 %
after porcelain firing
 98625 psi
@Strain 0.2 %
hardened
Elongation at Break 4.0 %hardened
 6.0 %after porcelain firing
Modulus of Elasticity 108 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature 25.0 - 500 °C
Melting Point 2030 - 2190 °F
Solidus 2030 °F
Liquidus 2190 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1470 °FPreheating Temp.
Casting Temperature 2460 °F
 
Component Elements PropertiesOriginal ValueComments
Gold, Au 78 %
Indium, In 4.0 %
Iridium, Ir 0.10 %
Palladium, Pd 8.0 %
Platinum, Pt 9.8 %
Tin, Sn 0.10 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wieland BioPorta G PFM Alloy
Johnson Matthey SC 850 Platinum w/ 15% Palladium Jewelry Alloy
Wieland Porta Geo Ti PFM Alloy
Wieland Porta REFLEX® PFM Alloy
Johnson Matthey HM Platinum w/ 5% Ruthenium Jewelry Alloy

NWIELAN03 / 19805

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.