MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds EPSILON® PRO Thixotropic epoxy coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Epoxy

Material Notes: Product Overview: Epsilon™ PRO is a thixotropic epoxy coating that self-thickens for brushing onto a variety of surfaces. Compared to original Epsilon™, Epsilon™ PRO offers a longer working time and cured epoxy is semi-rigid, offering better impact resistance. Mix ratio for Epsilon™ PRO is 2A:1B by volume (100A:44B by weight). A gram scale is not needed to use this product. Applied in thin layers, mixed material holds a vertical surface without sagging or slumping. Material wets out uniformly over different surfaces. Pot life is 22 minutes, with a re-coat time of 3 hours. All layers should be allowed to cure for 16 hours at 73° F / 23° C and can be accelerated with mild heat. Epsilon™ PRO is clear and can be easily colored using UVO™ or Ignite™ colorants. Cured coating has a gloss finish and can be sanded, primed and painted. Epsilon™ PRO is suitable for use as a protective, impact resistant coating for EPS or polyurethane foam. It can also be applied to plaster, concrete, wood and fabrics. This product is not sensitive to moisture / humidity and contains no VOC’s.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D-1475
Viscosity 4000 cPMixed; ASTM D-2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D-2240
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hourThin Film Tacky Recoat Time
 4.00 hourThin Film, Tack Free Time
 16.0 hour
 35.0 minThin Film Working Time
Pot Life 22.0 minASTM D-2471
 
Descriptive Properties
ColorClear Amber
Mix Ratio100A:44Bby weight
 2A:1Bby volume
Specific Volume25[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN206 / 296907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.