MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baypreg® F Polyurethane, Mat Reinforced Sandwich
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baypreg F system is a two component polyurethane system used in compression molding.

Properties / Applications: Baypreg F system is a two component polyurethane system used in compression molding of natural fiber mats alone, or fiber-reinforced sandwich panels to produce a variety of automotive parts. Some identified applications include door panels, sunshades, spare tire covers, load floors, etc. The Baypreg F system provides lightweight alternatives to ABS, PP, SMC, and wood products while demonstrating very high flexural stiffness and excellent thermal properties. Baypreg F system offers very diverse properties over a wide range of part thicknesses and densities while still providing cost effective substrate parts when combined with reinforcing materials. As with any product, use of the Baypreg F system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.250 g/ccASTM D792
 1.05 g/ccPolyol Blend (Component B)
 1.21 g/ccIsocyanate (Component A)
Viscosity 350 cPIsocyanate (Component A)
 800 cPPolyol Blend (Component B)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.0 MPaASTM D638
Flexural Strength 14.0 MPaASTM D790
Flexural Modulus 3000 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µin/in-°FASTM D696
Flash Point 160 °CPolyol Blend (Component B)
 223 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 100 - 120 °C
 
Descriptive Properties
AppearanceBlack liquidPolyol Blend (Component B)
 Dark brown liquidIsocyanate (Component A)
Content28.5%NCO, Isocyanate (Component A)
Hydroxyl number[KOH/g], Polyol Blend (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polynt BMC 580 Bulk Molding Compound Green Compound With Natural Fiber
Kareline Oy PPMS5050 Natural Fiber Reinforced Polypropylene for injection molding
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced

PCOVEST0217 / 202000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.