MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Weifang Tianrui Chemical IM-30 Acrylic Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Introduction: Impact modifier AIM product line is a generation of coreshell acrylic copolymer, the core layer of glass temperature is -54 ? - -30 ?. The series of impact modifier impact modifier and processing to improve performance in one, to increase the products of weathering and surface gloss, antiaging properties, especially suitable for outdoor use products, widely used in the profile, nontransparent sheet, plate, Pipe, PVC pipe, and other indoor and outdoor products and some of engineering plastics.

Application: High cold tolerance. It is used in some engineering plastics such as PMMA, PC and soon together in PVC rigid products which has a high requirement for cold tolerance .

Information provided by Weifang Tianrui Chemical Co., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Apparent Bulk Density 0.400 - 0.550 g/cc0.0145 - 0.0199 lb/in³
Particle Mesh Size 20 Mesh20 Mesh>98% Granularity (percent of pass)
 
Descriptive Properties
AppearanceWhite Freely Flowing Powder
Core glass transition temperature>-54°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEIFTC043 / 320556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.