MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Mineral Filled

Material Notes: Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding Resin

Former Eurostar product. Eurostar has been acquired by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 0.60 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 5.0 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaDAM; ISO 527-2
Elongation at Break 2.8 %DAM; ISO 527-2
Tensile Modulus 7500 MPaDAM; ISO 527-2
Flexural Strength 120 MPaDAM; ISO 178
Flexural Modulus 6800 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
 27.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched 30.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 30.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 3.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
UL RTI, Electrical 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 1.50 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 1.50 mm
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 1.50 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-2
@Thickness 1.50 mm
Oxygen Index 32 %DAM; EN ISO 4589-2
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 270 °CInjection
Middle Barrel Temperature 270 - 280 °CInjection
Front Barrel Temperature 270 - 285 °CInjection
Melt Temperature 270 - 285 °CInjection
Mold Temperature 60.0 - 90.0 °CInjection
Drying Temperature 75.0 - 85.0 °CInjection
Dry Time 4.00 - 6.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesBromine Free
 Flame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
Cheng Yu Plastic FRCV100 Flame Retardant Nylon 66, 10% Mineral Reinforced
Celanese Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry)

PEUROST879 / 171893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.