MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Syndustrial® PAG Compressor Oil ISO Grade 100
Categories: Fluid; Lubricant; Polyglycol

Material Notes: Syndustrial PAG Compressor Oil is a premium quality, synthetic lubricant developed for use in centrifugal and oil-flooded rotary screw and rotary vane compressors processing natural gas, carbon dioxide, propane or other hydrocarbon gases. It is specially formulated to resist hydrocarbon dilution and oil absorption in this type of service. Syndustrial PAG Compressor Oil is formulated with synthetic polyalkylene glycol (PAG) base oils and carefully selected additives to provide long service life, excellent wear protection, resistance to washout and lubricant carryover, and protection against rust and corrosion. Special inhibitors help resist corrosion caused by hydrogen sulfide when processing sour gas. The combination of outstanding oxidation resistance and thermal stability at high temperatures, a very high viscosity index, and excellent low-temperature properties makes it suitable for year-round use over a wide temperature range. Syndustrial PAG Compressor Oil is highly resistant to hydrocarbon gas dilution and absorption into the gas stream. Solubility of gas in the oil causes reduced lubricant viscosity, which can result in cylinder scoring and high wear rates. Absorption of the oil into the gas stream causes high oil consumption and carryover into the process gas, and can cause depletion of the protective oil film on the cylinder walls. Resistance to gas dilution and oil absorption helps maintain proper viscosity and oil film thickness to protect against wear.

Applications:

  • Oil-flooded rotary screw and rotary vane compressors processing natural gas, carbon dioxide or other hydrocarbon gases
  • Centrifugal compressors processing propane refrigerant, including York centrifugal compressors where York Oil Q (ISO VG 46) or York Oil R (ISO VG 68) is recommended
Features/Benefits:
  • Highly resistant to dilution by hydrocarbon gases
  • Resists washout by condensed hydrocarbon liquids
  • Resists absorption into the gas stream and subsequent carryover of the lubricant downstream
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • High viscosity index and low pour point for use over a wide temperature range
  • High film strength for wear protection
  • Protects against rust and corrosion
  • Extended service intervals compared to conventional mineral oil-based lubricants
  • Compatible with commonly used seals, gaskets and hoses

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
Density 8.66 lb/gal
Viscosity Measurement 218Index
Saybolt Viscosity at 100°F 503 SUS
Saybolt Viscosity at 210°F 97.8 SUS
Kinematic Viscosity at 40°C (104°F) 100 cSt
Kinematic Viscosity at 100°C (212°F) 19.4 cSt
Oxidative Stability 35 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.34[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.510 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -36.0 °C
Flash Point 232 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5043 / 198296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.