MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ FR Resin BFL4000U Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN BFL4000U Polycarbonate (PC) is an injection moldable non-chlorinated/brominated, unfilled, flame retardant grade with high flow. It is UV stabilized, light reflective and has an MVR of 22 (300°C/1.2kg) and a UL94 V0@1.5mm.

Features: Flame Retardant,Reflective,Diffusive,UV Resistant,Non-Chlorinated,Non-Brominated,Good Processability,Aesthetics & Visual effects

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
Density 1.38 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 22 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 24 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.0 MPa5 mm/min; ISO 527
 47.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa5 mm/min; ISO 527
 54.0 MPa5 mm/min; ASTM D638
Elongation at Break 56 %5 mm/min; ASTM D638
 74 %5 mm/min; ISO 527
Elongation at Yield 5.0 %5 mm/min; ASTM D638
 6.0 %5 mm/min; ISO 527
Tensile Modulus 2040 MPa1 mm/min; ISO 527
 2240 MPa5 mm/min; ASTM D638
Flexural Strength 83.0 MPayield, 2 mm/min; ISO 178
 90.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2050 MPa1.3 mm/min, 50 mm span; ASTM D790
 2170 MPa2 mm/min; ISO 178
Izod Impact Notched 470 JASTM D256
 240 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 30.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 68.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 131 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 134 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 115 °C
@Thickness 3.20 mm
annealed; ASTM D648
 124 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 136 °CRate B/50; ASTM D1525
 137 °CRate B/50; ISO 306
 139 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 265 - 290 °C
Zone 2 260 - 280 °C
Zone 3 270 - 295 °C
Melt Temperature 270 - 295 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80477 / 288424

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.