MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid Prototyping and Rapid Manufacturing applications.

Vero Family: Opaque rigid materials offering toughness, dimensional stability and great detail visualization

Fields of Use: Consumer electronics, Toy, Telecommunications, Computers and Architecture fields, Jewelry applications

Information provided by Proto3000 for their protoyping engineering services.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.17 - 1.18 g/ccPolymerized; ASTM D792
Water Absorption 1.1 - 1.5 %
@Time 86400 sec
ASTM D570-98
Ash 0.23 - 0.26 %USP281
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73 - 76
Hardness, Shore D 83 - 86
Tensile Strength at Break 50.0 - 65.0 MPaASTM D638-03
Elongation at Break 10 - 25 %ASTM D638-05
Modulus of Elasticity 2.00 - 3.00 GPaASTM D638-04
Flexural Strength 75.0 - 110 MPaASTM D790-03
Flexural Modulus 2200 - 3200 MPaASTM D790-04
Izod Impact, Notched 20.0 - 30.0 J/mASTM D256-06
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °CASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °CASTM D648-07
Glass Transition Temp, Tg 52.0 - 54.0 °CDMA, E

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® VEROGRAY Rigid Opaque 3D Printing Polymer
AISI 1018 Steel, hot rolled, quenched, and tempered
Proto3000 Objet VeroClear FullCure810
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer
Proto3000 PC-ABS Fused Deposition Modeling Polymer

PPROTO937 / 133137

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.