MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Feature: Injection Molding, TBBA-free Flame Retardant, Low Flow

Application: Electric/Electronic Applications (TV, Monitor Housing) IT/OA device

CAS No. 9003-56-9, 84852-53-9 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Maximum Moisture Content 0.0100.010Extrusion Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9999ASTM D785
Tensile Strength, Yield 42.2 MPa
@Thickness 3.20 mm
6120 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 20 %
@Thickness 3.20 mm
20 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield >= 5.0 %
@Thickness 3.20 mm
>= 5.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Tensile Modulus 2.16 GPa
@Thickness 3.20 mm
313 ksi
@Thickness 0.126 in
1 mm/min; ASTM D638
Flexural Yield Strength 66.7 MPa
@Thickness 6.40 mm
9670 psi
@Thickness 0.252 in
15 mm/min; ASTM D790
Flexural Modulus 2.35 GPa
@Thickness 6.40 mm
341 ksi
@Thickness 0.252 in
15 mm/min; ASTM D790
Izod Impact, Notched  1.77 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
3.31 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 2.45 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
4.59 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  0.686 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
1.29 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 0.785 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
1.47 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 6.40 mm
203 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
@Thickness 6.40 mm
185 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 94.0 °C
@Load 5.00 kg
201 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=2.00 mm
V-0
@Thickness >=0.0787 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Zone 1 170 - 190 °C338 - 374 °FExtrusion Molding
Zone 2 180 - 200 °C356 - 392 °FExtrusion Molding
Zone 3 200 - 220 °C392 - 428 °FExtrusion Molding
Zone 4 200 - 220 °C392 - 428 °FExtrusion Molding
Adapter Temperature 200 - 230 °C392 - 446 °FExtrusion Molding
Die Temperature 200 - 230 °C392 - 446 °FExtrusion Molding
Melt Temperature 200 - 230 °C392 - 446 °FExtrusion Molding
Roll Temperature 60.0 - 90.0 °C140 - 194 °FBottom, Extrusion
 70.0 - 90.0 °C158 - 194 °FMiddle, Extrusion
 70.0 - 100 °C158 - 212 °FTop, Extrusion
Drying Temperature 70.0 - 80.0 °C158 - 176 °FExtrusion Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical BM662 ABS, Heat Resistance
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
LG Chemical AF308 ABS, Flame Retardant
LG Chemical AF312 ABS, Flame Retardant
LG Chemical AF312A ABS, Flame Retardant

PLAY087 / 148095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.