MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Prevail® 3150 ABS + Polyurethane
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyurethane Alloy; Polyurethane, TP

Material Notes: PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used for applications ranging from flexible bumper fascias to sports equipment components. It is easy to process and is paintable without the need for a primer.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM Data
Melt Density 0.970 g/cc0.0350 lb/in³
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/in
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 27.6 MPa4000 psiASTM Data
Tensile Strength, Yield 24.1 MPa3500 psiASTM Data
Elongation at Break 180 %180 %ASTM Data
Elongation at Yield 16 %16 %ISO Data
Tensile Modulus 0.745 GPa108 ksiASTM Data
Izod Impact, Notched NBNBASTM Data
 3.74 J/cm
@Temperature -50.0 °C
7.01 ft-lb/in
@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NBNBISO Data
 NBNBISO Data, Low Temp
Charpy Impact, Notched 4.15 J/cm²19.8 ft-lb/in²ISO Data, Low Temp
 11.0 J/cm²52.4 ft-lb/in²ISO Data
Instrumented Impact Total Energy  52.0 J
@Temperature 23.0 °C
38.4 ft-lb
@Temperature 73.4 °F
 64.4 J
@Temperature -30.0 °C
47.5 ft-lb
@Temperature -22.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 88.0 µm/m-°C
@Temperature 20.0 °C
48.9 µin/in-°F
@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 1.54 J/g-°C0.368 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °FUnannealed; ASTM Data
 93.0 °C199 °FAnnealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FUnannealed; ASTM Data
 84.0 °C183 °FAnnealed; ASTM Data
Vicat Softening Point 102 °C216 °F
 
Optical PropertiesMetricEnglishComments
Gloss 72 %72 %Gardner Gloss, 60°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin
Dow Retain® 8209 ABS + Polycarbonate
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound

PDW121 / 34352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.