MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Compuestos Dominicanos Polycom AM-05495 PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance.

Applications: Wire covering for fence

Appearance: Natural pellets

Information provided by Compuestos Dominicanos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 - 1.39 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 86 - 88
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 2850 psiASTM D412
Elongation at Break 315 %ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary PVC FM1R Polyvinyl Chloride Thermoplastic
Colorite Polymers 9813 General Purpose Vinyl Compound
Overview of materials for PVC, Molded
Overview of materials for PVC, Extruded
Microcell Composite Company CELLwood® Thermal Plastic Elastomer

PPOLYC45 / 131344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.