MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton 278 Super Solv  (discontinued **)
Categories: Fluid

Material Notes: Description: Chesterton® 278 Super Solv is the strongest based cleaner in the Chesterton line. It is designed for those applications where only chlorinated solvents or aromatics previously worked. It will remove most adhesives, epoxies, resins, and tars. Chesterton 278 Super Solv will even attack baked on gums and polymers. Chesterton 278 Super Solv was formulated with the dual goals of strength and safety. This is evidence by several of the products’ features: 1) A flash point of 107°C (225°F). Risk of flammability when using Chesterton 278 Super Solv is considerably minimized. 2) No Chlorinated solvents – no ozone depleting potential and none of the health risks associated with such solvents. 3) Low aromatic content – the raw materials used in 278 Super Solv are non naphthenic but rather based on the synergistic cleaning effect of several polar and non-polar solvents. Chesterton 278 Super Solv can be used in the plant with confidence that virtually all the most difficult industrial soils will be attacked. Yet work safety and the environment will not be compromised.

Features:

  • Low Aromatic Content
  • Low Evaporation Rate
  • Safe For Use On All Metals
  • Dissolves Resins, Viscous Polymeric Materials, Epoxies, Adhesives
  • Contains No Ozone Depleting Substance.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
Volatiles 100 %
 
Thermal PropertiesOriginal ValueComments
Flash Point 107 °CPensky Martens; ASTM D93-85, DIN 51 755
 
Descriptive Properties
AppearanceClear, transparent liquid
Aromatic Content<0.5%(C8+)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTCHS061 / 138173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.