MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 8000/20 A/B US Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 8000/20 A/B US is a pourable, two component, addition-curing silicone rubber with short curing time and low hardness Shore A.

Special features:

  • fast cure at elevated temperature
  • pourable
  • low hardness Shore A
  • very low compression set
Application: Fabrication of soft copy and printer rollers by molding.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccComponent A; DIN 53497 A
 1.20 g/ccComponent B; DIN 53497 A
 1.20 g/cccured; DIN 53497 A
Viscosity 20000 cPComponent B; ISO 3219
 50000 cPComponent A; ISO 3219
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20cured; DIN 53505/ISO 868
Tensile Strength at Break 4.00 MPacured; DIN 53504S1/ISO 37
Elongation at Break 500 %cured; DIN 53504S1/ISO 37
Compression Set 10 %
@Temperature 175 °C,
Time 79200 sec
DIN 53517
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
Postcuring 2h/200°C
 
Descriptive Properties
AppearanceBeigeComponent B
 RedComponent A
 Redcured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9179 / 204708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.