MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Polystyrol 165 H GR 2 PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.

Applications: In blends with high impact Polystyrene or Styrolux; thermoformed articles for high impact resistant packagings of dairy products, breakers for cold beverages. As material for physically or chemically foamed sheet, eg. for meat trays or labels.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.045 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62
Moisture Absorption at Equilibrium <= 0.10 %23°C/50% RH; ISO 62
Melt Flow 3.553 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 150 MPa
@Load 36.5 kg,
Time 30.0 sec
ISO 2039-1
Tensile Strength at Break 52.0 MPaISO 527-1/-2
Elongation at Break 2.0 %ISO 527-1/-2
Tensile Modulus 3300 MPaISO 527-1/-2
Flexural Strength 86.0 MPaISO 178
Shear Modulus 1.40 GPaISO 6721-2
Charpy Impact Unnotched <= 25.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 1e+6 Hz
IEC 60250
 2.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 135 kV/mmK20/P50; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °CISO 75-1/-2
Vicat Softening Point 89.0 °CVST/B/50; ISO 306
 97.0 °CVST/A/120; ISO 306
Flammability, UL94 HB
@Diameter 1.60 mm
IEC 60695-11-10
 HB
@Diameter 3.18 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 240 °CFlat film
 180 - 280 °CInjection Molding
Mold Temperature 10.0 - 60.0 °CInjection Molding
 
Descriptive Properties
ColorCrystal Clear 00013
Commercial StatusEurope
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond TR 5000
Total PSC 500 Polystyrene
BASF Polystyrol® 165 H Polystyrene (Europe)
Chevron Phillips EA3025 Crystal Polystyrene
INEOS Styrolution PS 116 N/L GPPS

PBASG0625 / 132258

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.