MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAPET white Polyethylene terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes:
  • very good chemical resistance
  • resistant to cleaning agents
  • excellent wear properties
  • excellent strength and stiffness
  • low moisture absorption
  • improved surface hardness
  • resistance against high energy radiation
Target Industries:
  • food engineering
  • food processing
  • engineering for beverage filling systems
  • packaging and paper machinery
  • semiconductor technology
  • printing machines
  • mechanical engineering
  • pharmaceutical industry

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³
Moisture Absorption 0.500 %0.500 %saturation; ASTM D570
 0.0400 %
@Time 86400 sec
0.0400 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393ASTM D785
Hardness, Rockwell R 125125ASTM D785
Tensile Strength, Yield 68.9 MPa10000 psiASTM D638
Elongation at Break 12 %12 %ASTM D 638
Elongation at Yield 4.0 %4.0 %ASTM D 638
Modulus of Elasticity 3.24 GPa470 ksiASTM D638
Flexural Strength 107 MPa15500 psiASTM D790
Flexural Modulus 3.24 GPa470 ksiASTM D790
Compressive Yield Strength 96.5 MPa
@Strain 10 %
14000 psi
@Strain 10 %
ASTM D695
Compressive Strength 24.8 MPa
@Strain 1 %
3600 psi
@Strain 1 %
ASTM D695
Compressive Modulus 2.38 GPa345 ksiASTM D695
Izod Impact, Notched 0.283 J/cm0.530 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.25
@Pressure 0.276 MPa
0.25
@Pressure 40.0 psi
50 fpm; ASTM D3702
Coefficient of Friction, Static 0.190.19ASTM D3702
K (wear) Factor 423 x 10-8 mm³/N-M210 x 10-10 in³-min/ft-lb-hrAgainst Steel, 40 psi, 50 fpm; ASTM D 3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.4
@Frequency 60 Hz
3.4
@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm399 kV/inASTM D149
Dissipation Factor 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.2 µm/m-°C39.0 µin/in-°FASTM D696
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°F
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°F
Melting Point 254 °C490 °F
Maximum Service Temperature, Air 110 °C230 °FLong Term
 160 °C320 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 116 °C240 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °FASTM D648
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8195 / 319123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.