MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR Body Filler Talc for Polyester Filler
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyester compounds where consistent viscosity is critical and inherent low oil absorption provides higher filler loadings. Gel Talc and Body Filler talcs are platy, hydrophobic and non-abrasive.
Body Filler talc is designed to allow the formulator to achieve maximum pigment/binder ratios.

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.78 g/cc
Bulk Density 29.0 lb/ft³Loose
 69.0 lb/ft³Tapped
Brightness 92 %Hunter Y, Rd value, dry
Oil Absorption 24 %g oil/100 g filler; ASTM D281
Fineness 2.0Hegman Fineness; ASTM D1210
Moisture Absorption at Equilibrium <= 0.30 %
Loss On Ignition 17 %
Particle Size 1.8 µm@ 10%
 8.5 µmD50
 30 µm@ 98%
pH 9.0
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 1.0
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 1.0 %
CaO <= 13 %
Fe2O3 <= 1.0 %
MgO 24 %
SiO2 46 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR CLEAR-BLOC® 80 Antiblock Talc
CIMBAR NANO-FLEX® Talc - D for TPO Applications
CIMBAR FlexTalc® 610 Ultrafine Talc for TPO Applications
CIMBAR FlexTalc® 610D Ultrafine Talc for TPO Applications, Densified
CIMBAR FlexTalc® 1222 Ultrafine Talc for TPO Applications

CIMBAR944 / 133426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.