MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes:

Information provided by Ravago

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ASTM D792
Water Absorption 1.3 %1.3 %24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in0.125 in, DAM; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Flexural Strength 40.7 MPa5900 psiASTM D790
Flexural Modulus 1.31 GPa190 ksiASTM D790
Izod Impact, Notched 1.33 J/cm2.50 ft-lb/in73°F; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Dielectric Constant 6.0
@Frequency 100 Hz
6.0
@Frequency 100 Hz
ASTM D150
Dielectric Strength 21.7 kV/mm550 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C160 °FUnannealed; ASTM D648
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
BK
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
BK
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
NC
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
NC
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 293 °C520 - 560 °F
Mold Temperature 48.9 - 93.3 °C120 - 200 °F
Drying Temperature 73.9 °C165 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content 0.20 %0.20 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Screw Speed 40 - 140 rpm40 - 140 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond)
Avient Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66)
Solvay N1000 Nylon Mesh
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)

PENTA093 / 36130

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.