MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baytec® 505 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Baytec 505 is a diethyltoluenediamine (DETDA), an aromatic diamine.

Properties / Applications: Baytec 505 ’s primary application is a chain extender for use in RIM-processed polyurethanes. It is typically blended with other B-side components by the customer. Baytec 505 chain extender offers easier mold release, faster cycle times, and better heat distortion resistance than is available with traditional glycol-based chain extenders. As with any product, use of Baytec 505 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/cc
 0.875 g/cc
@Temperature 200 °C
 1.00 g/cc
@Temperature 50.0 °C
Viscosity 326 cP
 25 cP
@Temperature 100 °C
 125 cP
@Temperature 50.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point 160 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %
 
Component Elements PropertiesOriginal ValueComments
Nitrogen, N 15.5 - 15.9 %
 
Descriptive Properties
AppearanceAmber liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ZEON HyTemp® ZFC-65 Polyacrylate Curative
ZEON HyTemp® SC-75 Polyacrylate Curative
Evonik VESTAGON® B 31 Colorant

PCOVEST0230 / 202013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.