MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Achieve™ Advanced PP0502E1 Polypropylene Homopolymer
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Achieve™ Advanced PP0502E1 is a polypropylene homopolymer resin that provides excellent stiffness and heat tolerance performance while maintaining easy processing in blown film.  It has advantages as a blend component with polyethylene to produce films with outstanding mechanical properties and broad applicability.  Values generated below are based on 1.0 mil film thickness. 

Availability:  Africa & Middle East, Europe, Asia Pacific, North America.  Features:  Excellent processability, high heat resistance, high stiffness. 

Applications:  blown film extrusion, heavy duty sacks, food packaging, stand up pouches.  Appearance:  Natural Color.  Forms:  pellets.  Processing Method:  blown film.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 1.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 5600 psiExxonMobil Method
Film Tensile Strength at Yield, TD 3840 psiExxonMobil Method
Film Elongation at Break, MD 590 %ExxonMobil Method
Film Elongation at Break, TD 5.0 %ExxonMobil Method
Elmendorf Tear Strength MD 5.0 gASTM D1922
Elmendorf Tear Strength TD 70 gASTM D1922
Film Tensile Strength at Break, MD 11000 psiExxonMobil Method
Film Tensile Strength at Break, TD 5830 psiExxonMobil Method
1% Secant Modulus, MD 221000 psiExxonMobil Method
1% Secant Modulus, TD 205000 psiExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 325 °FPeak; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze >= 30 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP3746G Granular Homopolymer
ExxonMobil PP3546G Homopolymer Grade for Ultra-High Melt Flow Rate Nonwoven Applications
ExxonMobil Exceed™ PP6035G1 Polypropylene Homopolymer
ExxonMobil Exceed™ Flow PP6936G2 Polypropylene Homopolymer

PEX98967 / 238348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.