System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical KEYFLEX BT HB9255D Ester Type TPE
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester, TP
;
Polyester Thermoplastic Elastomer
Material Notes:
Description: TPC-ET, Blow Moldable, Medium Modulus, Black Color
Application: Air duct, Hose & Tubing
CAS: 37282-12-5, 24968-12-5 and 1333-86-4
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.16
g/cc
ASTM D792
Water Absorption
0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Maximum Moisture Content
0.010
Injection Molding
0.010
Extrusion Molding
Melt Flow
3.0
g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
47
ASTM D2240
Tensile Strength at Break
39.2
MPa
@Thickness 2.00 mm
50mm/min; ASTM D638
Elongation at Break
500 %
@Thickness 2.00 mm
50mm/min; ASTM D638
Flexural Modulus
2000
kg(f)/cm²
@Thickness 6.40 mm
15mm/min; ASTM D790
Izod Impact, Notched
15.0
kg-cm/cm
@Thickness 6.40 mm,
Temperature -40.0 °C
ASTM D256
NB
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
220
°C
Peak
Deflection Temperature at 0.46 MPa (66 psi)
70.0
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
220
-
240
°C
Injection Molding
Middle Barrel Temperature
230
-
250
°C
Injection Molding
Front Barrel Temperature
235
-
255
°C
Injection Molding
Nozzle Temperature
235
-
255
°C
Injection Molding
Zone 1
220
-
240
°C
Extrusion Molding
Zone 2
220
-
240
°C
Extrusion Molding
Zone 3
230
-
250
°C
Extrusion Molding
Zone 4
230
-
250
°C
Extrusion Molding
Adapter Temperature
230
-
250
°C
Extrusion Molding
Die Temperature
220
-
260
°C
Extrusion Molding
Melt Temperature
220
-
250
°C
Injection Molding
220
-
250
°C
Extrusion Molding
Mold Temperature
30.0
-
60.0
°C
Injection Molding
Drying Temperature
80.0
-
90.0
°C
Injection Molding
80.0
-
90.0
°C
Extrusion Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
3.00
-
4.00
hour
Extrusion Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LG Chemical KEYFLEX TO1088AV Olefin Type TPE
LG Chemical KEYFLEX BT GN7142F Ester Type TPE
LG Chemical KEYFLEX BT 5035D Ester Type TPE
LG Chemical KEYFLEX BT 3140D Ester Type TPE
LG Chemical KEYFLEX BT 3055D Ester Type TPE
PLAY445 / 148455
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.