MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 4311 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized under component file E40654. 04311 is available in black or brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.710 g/cc0.0257 lb/in³ASTM D1895
Density 1.48 g/cc0.0535 lb/in³ASTM D792
Water Absorption 0.267 %0.267 %ASTM D570
Linear Mold Shrinkage 0.0083 cm/cm0.0083 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7979ASTM D785
Tensile Strength, Ultimate 57.0 MPa8270 psiASTM D638
Elongation at Break 0.78 %0.78 %ASTM D638
Tensile Modulus 9.10 GPa1320 ksiASTM D638
Flexural Strength 89.0 MPa12900 psiASTM D790
Flexural Modulus 8.00 GPa1160 ksiASTM D790
Compressive Strength 177 MPa25700 psiASTM D695
Poissons Ratio 0.340.34ASTM D638
Shear Modulus 3.40 GPa493 ksiCalculated
Izod Impact, Notched 0.155 J/cm0.290 ft-lb/inASTM D256
Charpy Impact, Notched 0.165 J/cm²0.785 ft-lb/in²ASTM D256
Impact 8787J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.10e+11 ohm-cm4.10e+11 ohm-cmASTM D247
Dielectric Constant 5.25.2ASTM D150
Dielectric Strength 7.70 kV/mm196 kV/inStep by Step; ASTM D149
 11.0 kV/mm279 kV/inShort Time; ASTM D149
Dissipation Factor 0.0590.059ASTM D150
Arc Resistance 159 sec159 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 40.0 - 130 °C
27.8 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.490 W/m-K
@Temperature 100 °C
3.40 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 206 °C403 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 167 °C333 °FASTM D648
Flammability, UL94 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
Oxygen Index 29.4 %29.4 %ASTM D2863
Shrinkage 0.288 %0.288 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C-Glass Fiber, Generic
E-Glass Fiber, Generic
Plenco 1586 Polyester, Pellet, Injection Molded
Plenco 1581 Polyester, Pellet, Injection Molded
Plenco 1581 Polyester, Briquette, Transfer Molded

PLEL77 / 50649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.