MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Moplen HP552R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552R is a homopolymer typically used by customers in high speed production of staple fiber. Moplen HP552R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Features: Excellent spinnability; Excellent drawability; Anti-gas fading; Outstanding gloss and surface appearance

Applications: Staple Fiber for diaper and sanitary napkin; BCF/Multi-Filament: Automobile Interior stuffs; Industrial; Base resin for Master/Batch

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength, Yield 380 kg(f)/cm²ASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus 15000 kg(f)/cm²ASTM D790
Izod Impact, Notched 3.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 106 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex APEX® 75-9351A-102 Flexible Polyvinyl Chloride
LyondellBasell Moplen HP552R Polypropylene, Extrusion Grade
LyondellBasell Moplen EP548R Polypropylene, Impact Modified; Molded/Extruded
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
Celanese Hostaform® C 2521 LS POM, UV Resistant

PMIRAE41 / 53153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.