MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Selar® PT 8307 Polyester Barrier Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Selar® PT 8307 is a modified polyester copolymer resin in the high melt viscosity (HMV) series. The HMV modification changes the rheology of the melt and provides better processibility in extrusion operations. It can be processed in conventional extruders designed for polyolefins or polyesters.

Information provided by DuPont Packaging Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D1505
Moisture Vapor Transmission 1.10 cc-mm/m²-24hr-atmMocon Permatran W method
Oxygen Transmission 3.30 cc-mm/m²-24hr-atmASTM D3985
Viscosity Measurement 0.71Intrinsic viscosity per DuPont Method (in TFA/CH2 CH12)
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 2.76 GPa
@Diameter 3.17 mm
bar; ASTM D790
Secant Modulus, MD 2.10 GPaASTM D882
Secant Modulus, TD 2.025 GPaASTM D882
Impact 6.2J/mm Spencer Impact; ASTM D3420
Coefficient of Friction 0.35film/film; ASTM D1894
Elmendorf Tear Strength, MD 180 g/mil250 µm (10 mil) sheet; ASTM D1922
Film Tensile Strength at Break, MD 62.0 MPaASTM D882
Film Tensile Strength at Break, TD 59.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDSC/ASTM D3418
Glass Transition Temp, Tg 70.0 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze 0.20 %ASTM D1003
Gloss 100 %45°; ASTM D2457
 150 %20°; ASTM D2457
Transmission, Visible 80 %ASTM D1746
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 279 °CExtruder Die
Melt Temperature 271 - 282 °C
Drying Temperature 163 - 177 °C
Dry Time 6 - 8 hourto < 0.005% moisture.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyester Thermoplastic Elastomer
DuPont Selar® PT 4274 Polyester Barrier Resin
Soarus SoarnoL® DT2903 Ethylene Vinyl Alcohol Copolymer
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
DuPont Selar® PA 2072 Nylon Barrier Resin

PDUPL3 / 33659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.