MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: 27 mol % Ethylene.

Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas barrier properties.

EVAL™ is now produced as a part of the Kuraray product line.

Key Words: Ethylene Vinylalcohol
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D1505
Moisture Vapor Transmission 3.10 cc-mm/m²-24hr-atm7.87 cc-mil/100 in²-24hr-atm40°C, 90% RH
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm0.0102 cc-mil/100 in²-24hr-atm20°C; 65% RH; Permeability increases significantly at higher moisture content.
Melt Flow 3.9 g/10 min
@Load 2.16 kg,
Temperature 210 °C
3.9 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 104104ASTM D785
Tensile Strength, Yield 94.0 MPa13600 psi10%/min. ASTM D638
Film Elongation at Break, MD 200 %200 %Orientation not specified; ASTM D882
Elongation at Yield 6.0 %6.0 %10%/min. ASTM D638
Modulus of Elasticity 3.10 GPa450 ksiYoungs Modulus, ASTM D638, 10%/min.
Flexural Yield Strength 150 MPa21800 psiBending Strength; ASTM D790
Flexural Modulus 4.70 GPa682 ksiBending Elasticity; ASTM D790
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
Film Tensile Strength at Break, MD 72.0 MPa10400 psiOrientation not specified; ASTM D882
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.65.6Frequency Not Specified
Dissipation Factor 0.180.18Frequency Not Specified
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FBelow Tg
 105 µm/m-°C58.3 µin/in-°FAbove Tg
Specific Heat Capacity 2.40 J/g-°C0.574 BTU/lb-°F
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FFor EVAL F101
Melting Point 191 °C376 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FFor EP-F101
Glass Transition Temp, Tg 72.0 °C162 °FDynamic Viscoelasticity
 
Optical PropertiesMetricEnglishComments
Haze 1.8 %1.8 %Film; ASTM D1003
Gloss 85 %85 %45°; Film; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 240 °C<= 464 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Selar® RB 421 EVOH Barrier Resin
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin

PEVAL0 / 37290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.