MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Brandenburger BRA-GLA SI Thermal Insulation Board
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Silicone

Material Notes: Information provided by Brandenburger Isoliertechnik GmbH&Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.83 g/cc
Water Absorption 0.10 %DIN 53495
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 120 MPaEN 63
 37.0 MPa
@Temperature 200 °C
EN 63
Flexural Modulus 13.0 GPaEN 63
 6.90 GPa
@Temperature 200 °C
EN 63
Compressive Strength 450 MPaISO 604
 180 MPa
@Temperature 250 °C
 200 MPa
@Temperature 200 °C
ISO 604
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Thermal Conductivity 0.220 W/m-KDIN 52612
Maximum Service Temperature, Air 280 °CLong Term
 350 °CShort Term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brandenburger GL-P Thermal Insulation Board
Brandenburger S 4000 Thermal Insulation Board
Brandenburger GL-M Thermal Insulation Board
Brandenburger KV 3 Thermal Insulation Board
Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation

PBRAND02A / 27714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.