MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil PP7085E1 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applications like disposable houseware, consumer products, containers and rigid packaging applications.

Availability: Africa & Middle East and Europe

Features:

  • Antistatic
  • Controlled Rheology
  • High Flow
  • Nucleated
Uses:
  • Containers
  • Industrial Applications
  • Pails
  • Rigid Packaging
  • Tool/Tote Box
Processing Method: Injection Molding and Compounding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 75 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ISO 868
Tensile Strength, Yield 3340 psiISO 527-2/50
Elongation at Yield 5.0 %ISO 527-2/50
Tensile Modulus 167000 psiISO527-2/1
Flexural Modulus 163000 psiISO 178
Izod Impact, Notched (ISO) 2.60 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.90 ft-lb/in²
@Temperature -20.0 °C
ISO 179/1eA
 2.40 ft-lb/in²
@Temperature 0.000 °C
ISO 179/1eA
 3.60 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 322 °FISO 3146
Crystallization Temperature 253 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 180 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 122 °FISO 75-2/A
Vicat Softening Point 297 °FISO 306/A50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHX-006 Polypropylene Impact Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer

PEX99431 / 175667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.