MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BLUESTAR PBT 403M-G30 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: PBT, injection molding grade, 30% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 - 1.63 g/ccASTM D792
Moisture Absorption at Equilibrium 0.16 %50% RH; ASTM D570
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
Ash 28 - 34 %ISO 3451
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 105 MPa10mm/min; ASTM D638
Elongation at Break 1.8 %10mm/min; ASTM D638
Flexural Strength 165 MPa10mm/min; ASTM D790
Flexural Modulus 8000 MPa10mm/min; ASTM D790
Izod Impact, Notched (ISO) 7.50 kJ/m²ASTM D256
Izod Impact, Unnotched (ISO) 55.0 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.4
@Frequency 50 Hz
ASTM D150
Dielectric Strength 18.0 kV/mmin oil; ASTM D149
Dissipation Factor 0.020
@Frequency 50.0 - 60.0 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
Glow Wire Ignition Temperature 750 °C
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 °C
Melt Temperature 250 - 280 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 120 - 140 °C
Dry Time 3 - 4 hour
Injection Pressure 70.0 - 120 MPa
Back Pressure 6.00 - 18.0 MPa
Screw Speed <= 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 2300 G6 HR BK15116 30% Glass Filled PBT
Pearl Engineering PEPLPET B-105C PET Bottle Grade
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT

PBLUE902 / 135325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.