MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction IROGRAN A 92 E 4670 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a specially designed, flexible material with a broad processing window.

Performance Features:

  • High oil resistance
  • High production rate
  • Good melt flow
  • Easy coloring
  • Complies with FDA CFR 175.105 /177.2600
Applications:
  • Cable jacketing
  • Tubing
  • Technical extrusion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccInjection molded parts; ASTM D792
Linear Mold Shrinkage 0.0040 in/inInjection molded; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90Injection molded parts; ASTM D2240
Hardness, Shore D 38Injection molded parts; ASTM D2240
Tensile Strength at Break 36.0 MPaInjection molded parts; DIN 53504
Elongation at Break 600 %Injection molded parts; DIN 53504
100% Modulus 0.00850 GPa
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 0.0160 GPa
@Strain 300 %
Injection molded parts; DIN 53504
Rebound 1.21 %Bayshore
Tear Strength 460 pliInjection molded parts; ASTM D624
Abrasion 20mm3, Injection molded; DIN 53516
Compression Set 25 %
@Temperature 22.8 °C,
Time 86400 sec
Injection molded; ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
Injection molded; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 - 170 °C0.025" extruded film,
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester
Teknor Apex Laripur® LPR 9060EF Thermoplastic Polyurethane
Austin Novel Materials Texalan® 298A Polyester-based TPU
Covestro DUREFLEX® U073 TPU
Covestro DUREFLEX® PT1710S TPU

PHUQ100 / 159473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.