MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay FM® 10 Epoxy Syntactic Core
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: FM® 10 is a syntactic epoxy core material which is reinforced with hollow glass micro-balloons. FM 10 syntactic core is designed as a cost and/or weight saving alternative in the manufacture of thin [below 0.20 inches (5.1 mm) thick], stiffness critical composite panels. FM 10 syntactic core is compatible with nearly all commercially available 350°F (177°C) epoxy advanced composites. FM 10 will co-cure with these composites without the use of an adhesive film with. FM 10 is supplied with a non-woven Kevlar® mat (aromatic polyamide fiber) which improves handling characteristics in addition to increasing the material’s flexural strength. The product is slightly tacky for ease of handling. The product is supplied in sheet or roll form between two layers of release paper.

Features & Benefits:

  • 350°F (177°C) service temperature
  • Replaces honeycomb core in lightweight panels
  • 350°F (177°C) co-cure with most epoxy advanced composites
  • Low density core
  • Radar transparent
  • Excellent strength-to-weight ratio
Applications: Thin composite panels where weight, cost and/or stiffness are critical

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 0.610 g/cc
Thickness 970 - 1070 microns
Storage Temperature <= 18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1600 psi
@Temperature -55.0 °C
Flatwise
 1740 psi
@Temperature 177 °C
Flatwise, 30 day exposure in 100% RH at 160°F (71°C)
 1800 psi
@Temperature 24.0 °C
Flatwise
 2100 psi
@Temperature 177 °C
Flatwise
 2260 psi
@Temperature 24.0 °C
Flatwise, Turbine oil at 75°F (24°C)
 2400 psi
@Temperature 24.0 °C
Flatwise, Jet fuel at 75°F (24°C)
 2680 psi
@Temperature 24.0 °C
Flatwise, Skydrol LD4 fluid at 160°F (71°C)
 2950 psi
@Temperature 24.0 °C
Flatwise, 30 day exposure in 100% RH at 160°F (71°C)
Compressive Strength 7000 psi
@Temperature 177 °C
Block
 7000 psi
@Temperature 177 °C
Block, 30 day exposure in 100% RH at 160°F (71°C)
 8280 psi
@Temperature 24.0 °C
Block, Turbine oil at 75°F (24°C)
 8660 psi
@Temperature 24.0 °C
Block, Jet fuel at 75°F (24°C)
 10000 psi
@Temperature 24.0 °C
Block
 10360 psi
@Temperature 24.0 °C
Block, Skydrol LD4 fluid at 160°F (71°C)
 11520 psi
@Temperature 24.0 °C
Block, 30 day exposure in 100% RH at 160°F (71°C)
 13500 psi
@Temperature -55.0 °C
Block
Shear Strength 2040 psi
@Temperature 177 °C
Horizontal Beam, 30 day exposure in 100% RH at 160°F (71°C)
 4500 psi
@Temperature 177 °C
Horizontal Beam
 7000 psi
@Temperature 24.0 °C
Horizontal Beam
 8280 psi
@Temperature 24.0 °C
Horizontal Beam, Turbine oil at 75°F (24°C)
 8640 psi
@Temperature 24.0 °C
Horizontal Beam, 30 day exposure in 100% RH at 160°F (71°C)
 8660 psi
@Temperature 24.0 °C
Horizontal Beam, Jet fuel at 75°F (24°C)
 9540 psi
@Temperature 24.0 °C
Horizontal Beam, Skydrol LD4 fluid at 160°F (71°C)
 11500 psi
@Temperature -55.0 °C
Horizontal Beam
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 300-2K Film Adhesive, psf 0.1 (489 gsm)
Solvay CYCOM® 985 Epoxy Neat Resin
SGL Carbon Group SIGRAFIL C® C25 S012 EPY Staple Carbon Fiber, Epoxy Sizing
SGL Carbon Group SIGRAFIL C® C25 S009 EPY Staple Carbon Fiber, Epoxy Sizing
SGL Carbon Group SIGRAFIL C® C25 P250 EPY Pelletized Carbon Fiber, Epoxy Sizing

PCYTED024 / 180326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.