MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Dehesive® 944 Silicone Release Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: DEHESIVE® 944 is a solvent-based addition crosslinkable silicone recommended for release coatings.

Special features:

  • medium release at low peel speeds
  • good release stability
  • excellent bath life
  • excellent anchorage to a wide variety of substrates
  • suitable for coating PP and PE films and PE-coated paper
The silicone component of DEHESIVE® 944 is contained in the positive lists of BfR XV and XXXVI/2 and FDA §175.300, §175.320, §176.170 and §176.180. However, for compliance of the release coating with the before mentioned regulations the product has to be appropriately cured using a suitable crosslinker and under observance of the limits for platinum. The solvent toluene has to be completely removed.

Application: DEHESIVE® 944 may be used for coating of PE-laminated paper, polyester films (PET) and papers.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccDIN 51757
Solids Content 30 %
Viscosity 20000 cPdynamic
 
Thermal PropertiesOriginal ValueComments
Flash Point 6.00 °CISO 13736
Ignition Temperature 535 °Cliquids

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Dehesive® 919 Silicone Release Coating
Wacker Dehesive® 915 Silicone Release Coating
Wacker Dehesive® 910 Silicone Release Coating
Wacker Dehesive® SFX 251 AMA® Silicone Release Coating
Wacker Dehesive® SFX 250 Silicone Release Coating

PWACK9069 / 204598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.