MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials N-Sil® RTV123 Silicone Modified Alkoxy Adhesive Sealants, Black  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.

Key Performance Properties:

  • Primerless adhesion to many metals and plastics
  • Non-corrosive to aluminum and steel per MIL-A-46146A+
  • Lower odor cure than conventional silicone sealants
  • UL recognition (refer to GE Silicones Tech Info Sheet CDS4320 for additional information)
  • One component
  • Cures at room temperature
  • Excellent electrical insulation properties
  • Retains elastomeric properties at temperatures of -60°C(-75°F) to 204°C(500°F) for short periods
  • Excellent weatherability, ozone and chemical resistance

Applications:

Typical applications include, but are not limited to, sealing vertical joints bonding dissimilar materials such as metal to plastic and glass to aluminum, electrical insulation of wires and terminals, and formed-in-place gasketing.

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30
Tensile Strength, Ultimate 1.72 MPa
Elongation at Break 350 %
Tear Strength 6.220 kg(f)/cm
Peel Strength 35.0 pliGlass
 40.0 pliAluminum, Cold Rolled Steel, Epoxy, Rigid PVC
 45.0 pliGlass Filled Polyester
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cm
Dielectric Constant 2.8
@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
Dissipation Factor 0.0016
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.210 W/m-K
Brittleness Temperature -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
Through, 50% RH
Tack-Free Time 0.333 hour
@Temperature 25.0 °C
50% RH
 
Descriptive Properties
Application rate500 g/min3.2 mm orifice @ 621 kPa
ColorBlack
ConsistencyThixotropic Paste

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White
Momentive Performance Materials N-Sil® RTV128 Silicone Modified Alkoxy Adhesive Sealants, Translucent
Momentive Performance Materials RTV123 Black Adhesive Sealant, General Purpose Paste
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant
Henkel Loctite® FASTGASKET® 5960 Flange Sealant

PGESIL016 / 41007

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.