MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 10% Glass Fiber Reinforced

Material Notes: Feature: Injection Molding, POM+GF10%, High Rigidity

Application: Casings of Pump and Pivot Bearings

CAS No. 66455-31-0 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Maximum Moisture Content 0.10Injection Molding
Linear Mold Shrinkage, Flow 0.0060 - 0.011 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 83ASTM D785
Tensile Strength, Yield 1000 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 5.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength 1300 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 50000 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 5.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 50.0 °C
@Thickness >=0.750 mm
UL RTI, Mechanical with Impact 50.0 °C
@Thickness >=0.750 mm
UL RTI, Mechanical without Impact 50.0 °C
@Thickness >=0.750 mm
Flammability, UL94 HB
@Thickness >=0.750 mm
 HB
@Thickness >=1.50 mm
 HB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 180 - 200 °CInjection Molding
Middle Barrel Temperature 190 - 210 °CInjection Molding
Front Barrel Temperature 200 - 220 °CInjection Molding
Nozzle Temperature 200 - 220 °CInjection Molding
Melt Temperature 210 - 220 °CInjection Molding
Mold Temperature 60.0 - 100 °CInjection Molding
Drying Temperature 90.0 - 110 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Back Pressure 0.000 - 4.02 MPaInjection Molding
Screw Speed 40 - 75 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
Polykemi AB POLYform POM C M90 GF30 Polyoxymethylene
Delrin Delrin® 577 BK000 POM-GF20
Delrin Delrin® 510GR NC000 POM-GF10

PLAY115 / 148123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.