MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey Argo-braze 49LM Trifoil Silver Brazing Alloy for Tungsten Carbide Brazing
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: This material is supplied as Trifoil. Trifoil consists of a layer of copper sandwiched by brazing alloy. The copper helps to absorb the stresses caused by the differential expansion rates, under heating, of carbides and most steel backings.

Information provided by Johnson Matthey.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 670 - 710 °C
Solidus 670 °C
Liquidus 710 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 27.5 %
Manganese, Mn 2.5 %
Nickel, Ni 0.50 %
Silver, Ag 49 %
Zinc, Zn 20.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze 502 Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze 49H Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze 40N Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze™ 49CN Tri-foil Silver Brazing Filler Metal

NJMMJ14 / 17620

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.