MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Description: Cell Cast Acrylic

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Water Absorption 0.20 %24 hr immersion
Water Absorption at Saturation 0.65 %26 day immersion
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 50ASTM D2583
Hardness, Rockwell M 98ASTM D785
Tensile Strength, Yield 11250 psiASTM D638
Elongation at Break 6.4 %ASTM D638
Tensile Modulus 450000 psiASTM D638
Flexural Strength 15250 psiASTM D790
Flexural Modulus 475000 psiASTM D790
Compressive Yield Strength 18000 psiASTM D695
Compressive Modulus 440000 psiASTM D695
Shear Strength 9000 psiASTM D732
Izod Impact, Notched 0.375 ft-lb/inASTM D882
Impact 18inches, Falling 0.5 lb Steel Ball Breakage Height; ASTM D256
Compression Set 0.75 %
@Temperature 50.0 °C
4000 psi, 24 hr (Compression Deformation); ASTM D621
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 0.350 BTU/lb-°F
@Temperature 25.0 °C
Dupont 900 (Therm. An. Cal.)
Thermal Conductivity 1.30 BTU-in/hr-ft²-°FCento-Fitch
Maximum Service Temperature, Air 180 °F
Deflection Temperature at 0.46 MPa (66 psi) 230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °FASTM D648
Flame Spread 1.2 in/minBurning Rate UL 94 HB; ASTM D635
Flash Point 830 °FSelf Ignition Temperature; ASTM D1929
Smoke Density 27% Smoke Density; ASTM D2843
Shrinkage 2.2 %Residual Shrinkage (Internal Strain) Polycast; ASTM D4802
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Haze <= 0.50 %As Cast; ASTM D1003
Transmission, Visible 92 %As Cast; ASTM D1003
UV Transmittance >= 80 %
@Wavelength 320 nm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 320 °FHot Forming Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite Optix® CA - 51 HF UVT General Purpose Acrylic Resin
Overview of materials for Acrylic, Cast
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin
Plaskolite West Optix® CA - 41 UVT General Purpose Acrylic Resin
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000

PSPAR045 / 68486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.