MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC/ABS Alloy, Flame Retardant, Standard Flow

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 25 - 50 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8200 psiASTM D638
Tensile Strength, Yield 8400 psiASTM D638
Flexural Strength 13500 psiASTM D790
Flexural Modulus 380 ksiASTM D790
Izod Impact, Notched 12.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 320 in-lbASTM D3029
 
Electrical PropertiesOriginal ValueComments
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 1.50 mm
UL 746
 15 - 30 sec
@Thickness 2.50 mm
UL 746
 60 - 120 sec
@Thickness 3.00 mm
UL 746
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
UL 746
 >= 120 arcs
@Thickness 2.50 mm
UL 746
 >= 120 arcs
@Thickness 3.00 mm
UL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 195 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 185 °FASTM D648
UL RTI, Electrical 140 °F
@Thickness 1.50 mm
UL 746
 140 °F
@Thickness 2.50 mm
UL 746
 140 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 140 °F
@Thickness 1.50 mm
UL 746
 140 °F
@Thickness 2.50 mm
UL 746
 140 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 140 °F
@Thickness 1.50 mm
UL 746
 140 °F
@Thickness 2.50 mm
UL 746
 140 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0 - 5VA
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 430 - 490 °F
Middle Barrel Temperature 450 - 510 °F
Front Barrel Temperature 470 - 530 °F
Melt Temperature 475 - 525 °F
Mold Temperature 120 - 180 °F
Drying Temperature 170 - 180 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.00150 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Texin® 260 Thermoplastic Polyurethanes (TPU)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer

PPOLYQ080 / 160596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.