MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omnia Plastica PVC Polyvinylchloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.

Features:

  • High chemical resistance
  • Higher stiffness compared to polyolefins
  • Easy machinability on mechanical tools. It can be hot welded
  • Colour: grey, ivory, red
Weak Point:

Compared to PP it has lower shock and temperature resistance. The high gravity reduces its cheapness.

Application:

  • Chemical: the main application of PVC is in the chemical industry, thanks to its high resistance to acids and alkali and to its rigidity. It is used for components such as valves, flanges, gears, etc. in the chemical, galvanic and petrochemical industries.
  • Food contact: it cannot be used in contact with food.
  • Electrical: good dielectric properties and weather resistance make it suitable for these applications.
  • Mechanical: it is also used for mechanical components in corrosive environments. Compared to polyolefins, it has a higher tensile stress.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.10 %50% relative humidity
Water Absorption at Saturation 0.10 %23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 97dry sample; ISO2039.2
Ball Indentation Hardness 75.0 MPaISO2039.1 DIN.53456
Tensile Strength at Break 55.0 MPaISO.527 DIN.53455
Elongation at Break 20 %ISO.527 DIN.53455
Tensile Modulus 2.60 GPaISO.527 DIN.53455
Compressive Strength 7.00 MPa1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched 1.50 J/cm²7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 0.400 J/cm²ISO179/3C DIN.53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmISO.93 DIN.53482
Dielectric Constant 3.0
@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 50.0 kV/mmISO.243 DIN.53481
Dissipation Factor 0.015
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.150 W/m-KDIN.52612
Melting Point 80.0 °C
Maximum Service Temperature, Air 60.0 °CContinuous; 5000 hours based on a tensile stress of 50% at 23° C.
 65.0 °Cshort period, no load
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO.75 DIN.53461
Minimum Service Temperature, Air -5.00 °Cimpact conditions and heavy loads not considered
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid
Colorite Polymers 2010 Rigid PVC
Colorite Polymers 2007 Rigid PVC
Colorite Polymers 2002 Rigid PVC

POMNIA37 / 55627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.