MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vyncolit 2920 W Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: Mineral and organic filled molding compound with good dimensional stability and heat resistance.

USES: Carburettor and intake manifold thermal insulator.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.750 - 0.850 g/ccPowder Density; ISO 60
Density 1.75 g/ccRelative Density; ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cmInjection Molding; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 - 50.0 MPaISO 527
Elongation at Break 0.65 - 0.75 %Tensile; ISO 527
Tensile Modulus 10.5 - 12.0 GPaISO 527
Flexural Strength 80.0 - 100 MPaAt Rupture; ISO 178
Flexural Modulus 6.00 - 8.00 GPaISO 178
Flexural Strain at Break 1.2 - 1.3 %ISO 178
Compressive Strength 200 - 230 MPaISO 604
Charpy Impact Unnotched 0.650 - 0.800 J/cm²ISO 179
Charpy Impact, Notched 0.200 - 0.300 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+10 - 1.00e+11 ohmDry; IEC 167
Dielectric Strength 25.0 kV/mmIEC 243
Comparative Tracking Index 175 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 - 40.0 µm/m-°C
@Temperature 20.0 °C
TMA
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C
@Temperature 20.0 °C
TMA
Deflection Temperature at 1.8 MPa (264 psi) 150 - 180 °CISO 75 Af
Deflection Temperature at 8.0 MPa 130 - 150 °CISO 75 C
Flammability, UL94 V-1
@Thickness 1.60 mm
 V-0
@Thickness 4.00 mm
Shrinkage 0.10 - 0.20 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
ISO typePF 2 C3
Main FillerMineral & Organic
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit X658 Novolac Phenolic
Vyncolit 3640 CG Novolac Phenolic
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound
Sumitomo Bakelite North America RX® 865M Novolac Phenolic
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate

PVYNC034 / 72242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.