MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ VX5022 PBT (Europe)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Density 1.39 g/ccISO 1183
Filler Content 20 %ASTM D229
Water Absorption 0.10 %23°C/sat; ISO 62
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Viscosity 215 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 - 0.0080 cm/cmSABIC method
 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cmSABIC method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 16 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 28 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 40 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 50 g/10 min
@Load 5.00 kg,
Temperature 266 °C
ASTM D1238
 50 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ISO 2039-2
Ball Indentation Hardness 205 MPaISO 2039-1
Tensile Strength at Break 110 MPa5 mm/min; ISO 527
 125 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 110 MPa5 mm/min; ISO 527
 125 MPa5 mm/min; ASTM D638
Elongation at Break 3.0 %5 mm/min; ASTM D638
 3.0 %5 mm/min; ISO 527
Elongation at Yield 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Tensile Modulus 7100 MPa1mm/min; ISO 527
 7300 MPa5 mm/min; ASTM D638
Flexural Strength 150 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 145 MPa1.3 mm/min, 50 mm span; ASTM D790
 150 MPa2 mm/min; ISO 178
Flexural Modulus 5800 MPa1.3 mm/min, 50 mm span; ASTM D790
 6300 MPa2 mm/min; ISO 178
Flexural Strain at Break 3.0 %2 mm/min; ISO 178
Izod Impact, Notched 80.0 J/mASTM D256
 80.0 J/m
@Temperature -30.0 °C
ASTM D256
 80.0 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Unnotched 650 J/mASTM D4812
 645 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²80*10*4; ISO 180/1U
 35.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 40.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 55.0 kJ/m²ISO 179/2C
 40.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 6.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 9.00 kJ/m²ISO 179/2C
 5.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 65.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
 >= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+16 ohmROA; IEC 60093
Dielectric Constant 3.1
@Frequency 50.0 - 60.0 Hz
IEC 60250
 3.3
@Frequency 1e+6 Hz
ASTM D150
 3.3
@Frequency 1e+6 Hz
IEC 60250
 3.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 16.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 28.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 28.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 31.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
 31.0 kV/mm
@Thickness 0.800 mm
in oil; ASTM D149
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 60250
 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.014
@Frequency 1e+6 Hz
ASTM D150
 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 VIEC 60112
 250 VIEC 60112
Hot Wire Ignition, HWI >= 120 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 24.3 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 24.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 40.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 40.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 40.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 68.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 100 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 112 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 180 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 180 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 120 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/50; ISO 306
 145 °CRate B/120; ISO 306
 145 °CRate B/50; ASTM D1525
 200 °CRate A/50; ASTM D1525
 200 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 HB
@Thickness 3.00 mm
UL 94
Oxygen Index 23 %ISO 4589
Glow Wire Test 750 °C
@Thickness 1.00 mm
IEC 60695-2-12
 850 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 230 - 245 °C
Zone 2 240 - 255 °C
Zone 3 245 - 265 °C
Melt Temperature 250 - 270 °C
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10313 / 243780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.