MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is based on the elements Carbon, Hydrogen, Oxygen, Silicon, and Calcium. Compounds based on these elements will therefore be the only significant constituents of the combustion fumes. Other elements my be present in concentrations less than 0.1%. Flame retardancy is conferred by an inorganic filler and a novel char forming additive

Casico FR4805 is intended to be used as a 90°C rated jacket for fixed building wires (installation cables) and all types of power cables. This product can be used in areas sensitive to smoke or corrosive and toxic combustion products. The principal feature of this product is the high physical strength and toughness. For small downsized cables the enhanced physical properties compensate for reduced cross sectional area. For most cable constructions Casico FR4805 has sufficient flame retardancy to satisfy single wire vertical burning tests. The product contains a UV stabilization system.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccCompound; ISO 1872-2/ISO 1183-D
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ASTM D2240
Tensile Strength, Yield 2755 psiCable At 50 mm/min; IEC 60811-1-1
Elongation at Break 600 %Cable; IEC 60811-1-4
Flexural Modulus 0.590 GPaISO 178
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+16 ohm-cmCompound; IE 600093
Dielectric Strength >= 60.0 V/milCompound; IEC 60243
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 29 %ISO 4589-A-IV/ISO 5660
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature >= 180 °C
Front Barrel Temperature >= 160 °C
Die Temperature >= 374 °F
Head Temperature >= 190 °C
 
Descriptive Properties
Average Rate of Heat Release, kW/m^2305ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)
Change of Tensile Properties20% maxIEC 60811-1-2, After Heat Ageing (100°C, 10 days)
 20% maxIEC 60811-1-2, After heat ageing (100°C, 7 days)
 20% maxNF c 32-62-2 Annexe 3, After UV ageing (1000 hours)
CO, kg/dm^30.026ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)
CO2, kg/dg^31.8ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)
Corrosivity of Combustion Fumes, µS/cm27IEC 60754-2
Heat of Combustion, MJ/dm^324.5ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)
Ignition Time, sec75ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)
Maximum Rate of Heat Release, kW/m^2445ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)
Pressure Test at High Temp, %35IEC 811-3-1, Cable - Pressure Test at High Temperature (115°C,6 hours)
 9IEC 811-3-1, Cable - Pressure Test at High Temperature(90°C, 4 hours)
Smoke Obscuration, m^2/dm^3529ISO 5660, Cone Calorimeter (heat flux 35 kW/m^2)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
Borealis Casico™ FR4803 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borealis Casico™ FR4804 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
A. Schulman Diamond DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE

PBOREA142 / 27449

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.