MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Vectra® K140 Liquid Crystal Polymer (LCP), 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³ISO 1183
Water Absorption 0.040 %0.040 %Immersion to equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.040 %0.040 %ISO 62
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
Linear Mold Shrinkage, Transverse 0.0020 cm/cm0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 160 MPa23200 psiISO 527
Elongation at Break 1.2 %1.2 %IEC 527
Tensile Modulus 20.0 GPa2900 ksiISO 527
Flexural Strength 245 MPa35500 psiISO 178
Flexural Modulus 18.0 GPa2610 ksiISO 178
Compressive Strength 127 MPa18400 psi1% Deflection, ISO 604
Compressive Modulus 18.0 GPa2610 ksiISO 604
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 93
Surface Resistance 1.00e+17 ohm1.00e+17 ohmIEC 93
Dielectric Constant  3.6
@Frequency 1e+7 Hz
3.6
@Frequency 1e+7 Hz
 4.1
@Frequency 1000 Hz
4.1
@Frequency 1000 Hz
IEC 250
Dissipation Factor  0.010
@Frequency 1e+7 Hz
0.010
@Frequency 1e+7 Hz
 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
IEC 250
Arc Resistance 140 sec140 sec
Comparative Tracking Index 175 V175 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  3.00 µm/m-°C
@Temperature -50.0 - 200 °C
1.67 µin/in-°F
@Temperature -58.0 - 392 °F
 3.00 µm/m-°C
@Temperature -58.0 - 390 °C
1.67 µin/in-°F
@Temperature -72.4 - 734 °F
CTE, linear, Transverse to Flow  79.0 µm/m-°C
@Temperature -50.0 - 200 °C
43.9 µin/in-°F
@Temperature -58.0 - 392 °F
 79.0 µm/m-°C
@Temperature -50.0 - 200 °C
43.9 µin/in-°F
@Temperature -58.0 - 392 °F
Melting Point 320 °C608 °FISO 3146
Maximum Service Temperature, Air 130 °C266 °FGeneric Rating for Vectra LCP
Deflection Temperature at 1.8 MPa (264 psi) 217 °C423 °FISO 75/A
UL RTI, Electrical 130 °C266 °FGeneric Rating for Vectra LCP
UL RTI, Mechanical with Impact 130 °C266 °FGeneric Rating for Vectra LCP
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA S135 LCP, 35% Glass Reinforced
Celanese Vectra® K130 Liquid Crystal Polymer (LCP), 30% Glass Reinforced
Aluminum 5052-H32
Copper, Cu; Cold Drawn
Silicon, Si

PHCU87 / 45827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.