MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay FM® 377S Adhesive Film, psf 0.08 (391 gsm)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 377 film adhesive is a 350°F (177°C) cure modified epoxy designed for continuous services at 350°F (177°C). FM 377 film adhesive provides outstanding durability in bonding metallic and non-metallic substrates, and in the co-cure or secondary bonding of composites structures. FM 377 adhesive exhibits excellent structural performance from -67°F to 350°F (-55°C to 177°C). FM 377 adhesive is manufactured as a supported film with a knit carrier or as an unsupported film. The unsupported version can be easily reticulated on honeycomb core or perforated metal.

Features & Benefits:

  • Designed for bonding metallic, non-metallic and sandwich structures
  • Excellent combination of high peel strength and high 350°F (177°C) shear strength
  • Designed for continuous service at 350°F (177°C)
  • Superior performance in co-cure or secondary bonding of composite structures
  • Easily reticulated on core or perforated metal for nacelle bonding applications
  • 30 days shop life at 75°F (24°C)
Applications:
  • Bonding metallic, non-metallic and sandwich structures
  • Co-cure and secondary bonding of composite structures

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 485 psi
@Temperature 177 °C
Flatwise, Honeycomb Specimens
 490 psi
@Temperature 177 °C
Flatwise, After 1000 hr aging at 350°F (177°C), Honeycomb Specimens
 1210 psi
@Temperature 24.0 °C
Flatwise, Honeycomb Specimens
Shear Strength 800 psiBeam, Honeycomb Specimens
 1845 psi
@Temperature 177 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 28 days
 1900 psi
@Temperature 177 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 63 days
 1950 psi
@Temperature 177 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 14 days
 1985 psi
@Temperature 177 °C
Blister, Metal-to-Metal
 2050 psi
@Temperature 177 °C
Wide Area Lap, Prebond Film Exposure at 24°C
 2110 psi
@Temperature 177 °C
Blister, after 1000 hrs at 350°F, Metal-to-Metal
 3500 psi
@Temperature -55.0 °C
Blister, Metal-to-Metal
 3595 psi
@Temperature -55.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C
 3685 psi
@Temperature -55.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 14 days
 3695 psi
@Temperature -55.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 63 days
 3700 psi
@Temperature 24.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 63 days
 3730 psi
@Temperature 24.0 °C
Blister, Metal-to-Metal
 3780 psi
@Temperature 24.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 14 days
 3835 psi
@Temperature 24.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C
 3845 psi
@Temperature -55.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 28 days
 3870 psi
@Temperature 24.0 °C
Wide Area Lap, Prebond Film Exposure at 24°C, for 28 days
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °Ccontinuous
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorGrey
Honeycomb Sandwich Peel133 Nm/mHoneycomb Specimens
 66 Nm/mPrebond Film Exposure at 24°C, for 63 days
 69 Nm/mPrebond Film Exposure at 24°C, for 28 days
 74 Nm/mPrebond Film Exposure at 24°C
 80 Nm/mPrebond Film Exposure at 24°C, for 14 days
Metal-to-Metal Climbing Drum Peel155 Nm/mPrebond Film Exposure at 24°C
 156 Nm/mMetal-to-Metal
 160 Nm/mPrebond Film Exposure at 24°C, for 14 days
 164 Nm/mPrebond Film Exposure at 24°C, for 28 days
 164 Nm/mPrebond Film Exposure at 24°C, for 63 days

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 377U psf 0.055 (269 gsm) Adhesive Film
Overview of materials for Epoxy Adhesive
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive
Atom Adhesives AA-BOND FDA16 Epoxy Adhesive
Armstrong A-2/H20 Epoxy Adhesive

PCYTED120 / 180422

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.