MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hapco Hapflex 791-5 Semi-rigid urethane elastomers
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: The Hapflex 700/800 series products are known for clear/colorless appearance and their durability. When post-cured, these products are virtually unbreakable. Living hinges, protective coverings, fixtures, forming dies, foundry patterns, and core boxes are just a few examples this series’ uses.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D-4669
Viscosity 4000 cP4000 cPASTM D-4878
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D-2240
Tensile Strength 24.3 MPa3530 psiASTM D-638
Elongation at Break 420 %420 %ASTM D-638
Izod Impact, Notched NBNBASTM D-256
Izod Impact, Unnotched NBNBASTM D-256
Tear Strength 61.4 kN/m350 pliASTM 624 Die C
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 240 min
@Thickness 3.17 mm
2.00 - 4.00 hour
@Thickness 0.125 in
Demold
Gel Time 5.00 min
@Load 0.100 kg
5.00 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)Colorless
Mix Ratio100:15Volume
 100:15Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO130 / 317189

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.