MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.

Typical Applications: Seals, compressors, pumps, bearings

Information provided by SGL Carbon Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/cc
Open Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105Ball Size/Load - 5/100
Modulus of Elasticity 1100 ksi
Flexural Strength 13000 psi
Compressive Strength 29500 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 350 °FIn oxygen
Maximum Service Temperature, Inert 204 °CReducing Atm.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SGL Carbon Group Ridurid® EK 60 High Performance Graphite Filled Plastic
Epoxyset Epoxiohm EO-21 Electrically Conductive Epoxy Adhesive
Epoxy Technology EPO-TEK® 430 Epoxy
Cookson Group Plaskon® ALP-2 (188.pcs03) Thin Package Encapsulant
Sumitomo Bakelite Sumikon® PM-TX110 Phenolic Resol

PSGL04 / 67278

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.