MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Leaded Brass, Copper Alloy, UNS C35350, H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Good Suitability – Soldering, Brazing; Poor Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed

Applicable Specifications: Rod, Bar & Shapes – ASTM B453/B453M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.301 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 140
@Load 0.500 kg
Tensile Strength 50.0 - 69.0 ksi
 64.0 ksiTypical
Tensile Strength, Yield 39.0 - 64.0 ksi0.2% Offset
 60.0 ksi0.2% Offset, Typical
Elongation at Break 25 %
Tensile Modulus 17600 ksi
Modulus of Rigidity 4560 ksi
Poissons Ratio 0.26
Fatigue Strength 25000 psi
@# of Cycles 1.00e+8
Machinability 88 %
Impact Test 21.0 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000750 ohm-cm23% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.2 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 61.3 BTU-in/hr-ft²-°F
Melting Point 1578 - 1654 °F
Solidus 1578 °F
Liquidus 1654 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 61 - 63 %
Iron, Fe <= 0.40 %
Lead, Pb 2.0 - 4.5 %
Nickel, Ni <= 0.30 %
Phosphorus, P 0.050 - 0.20 %
Tin, Sn <= 0.60 %
Zinc, Zn 31.4 - 37 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC35350x1 / 291863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.