MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D1157 ES D SBS Linear Block Copolymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Kraton D1157 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. Kraton D1157 E is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Kraton D1157 ES is supplied as porous pellets dusted with amorphous silica.

Information provided by Kraton Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 2781
Bulk Density 0.400 g/ccASTM D1895 Method B
Melt Flow 3.5 - 6.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Ash 0.10 - 0.40 %ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 15.0 sec
Compression molded slab; ASTM D2240
Tensile Strength 28.0 MPaCast Film; ISO 37
Elongation at Break 800 %Cast Film; ISO 37
300% Modulus 421 psi
@Strain 300 %
Cast Film; ISO 37
 
Descriptive Properties
Antioxidant>=0.15Test Method KM 08
Polystyrene Content (%m)28.5 to 30.5Test Method KM 03
Total Extractables<=1 %mTest Method KM 05
Volatile Matter (%m)<= 0.3KM 04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1157 A D SBS Linear Block Copolymer
KKPC KOSYN KTR 601 Thermoplastic Elastomer (TPE)
KKPC KOSYN KTR 201 Thermoplastic Elastomer (TPE)
KKPC KOSYN KTR 101 Thermoplastic Elastomer (TPE)
Dow Engage® Polyolefin Elastomer

PKQZ9005 / 239869

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.