MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovako 94CrMo5-2* 821L Steel, Q/T (bainite)
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Ovako 821L is a through hardening bearing steel intended for rolling contact and other high fatigued applications. In the hardened condition the high hardness, high strength and high cleanliness provides the steel with the right properties to withstand high cycle, high stress fatigue. Ovako 821L is mainly used for small and medium sized bearing components. It is also regularly used for other machine components that require high tensile strength and high hardness.

BQ-Steel:(Bearing Quality) is a bearing quality clean steel optimized for fatigue strength by a strict control of steel cleanliness. BQ-steel is also ideal for new design solutions in a wide array of demanding applications outside the bearing industry that require longer performance and higher loads. The BQ-steel offer is the result of the Ovako clean steel program. Purity of production means that the material has significantly smaller inclusions compared to conventional steel and, as a result, the fatigue strength of the steel is increased dramatically. Use of the material allows components to be manufactured in smaller sizes. The BQ-steel has for decades been the problem-solver.

Information provided by Ovako

Key Words: 100Cr6, 52100, 100 C 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 59All formats
Tensile Strength 2200 MPaAll formats
Tensile Strength, Yield >= 2000 MPaAll formats
Elongation at Break 7.0 %All formats
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 115 °CMS
 750 °CAC1
 750 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.94 - 1.0 %
Chromium, Cr 1.3 - 1.5 %
Iron, Fe 96.5 - 97.21 %As Balance
Manganese, Mn 0.25 - 0.45 %
Molybdenum, Mo 0.20 - 0.23 %
Nickel, Ni <= 0.15 %
Phosphorus, P <= 0.015 %
Silicon, Si 0.10 - 0.15 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako 100Cr6 803J Steel, Q/T (bainite)
Ovako 94CrMo5-2* 821L Steel, Q/T (martensite)
Ovako 100Cr6 ISO 683-17 (ref) Steel, +A, Round bar
Ovako 100Cr6 803J Steel, Q/T (martensite)
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)

NOVAKO378 / 234677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.