MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler

Material Notes: 30% Carbon Fiber Reinforced Polyphenylene Sulfide

Information provided by Oxford Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Filler Content 30 %
Water Absorption 0.040 %ASTM D570
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27000 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 33.0 ksiASTM D790
Flexural Modulus 2500 ksiASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 500 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS)
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
Polyram Polytron P60B11 Homopolymer Polypropylene, Chemically Coupled 60% LGF
RTP Company ESD 283 TFE 5 HS Nylon 6/6 (PA); Carbon Fiber - Electrically Conductive - PTFE Lubricated - Heat Stabilized
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber

POX22 / 55871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.