MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lupolen 5236 HX HDPE, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Impact Grade

Material Notes: Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.

Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³
Water Absorption 0.010 %0.010 %
Moisture Absorption at Equilibrium 0.10 %0.10 %
Linear Mold Shrinkage, Flow 0.023 cm/cm0.023 in/in
Linear Mold Shrinkage, Transverse 0.024 cm/cm0.024 in/in
Melt Flow 3.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 9.0 %9.0 %
Tensile Modulus 1.10 GPa160 ksi
Tensile Impact Strength 90.0 kJ/m²42.8 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.4
@Frequency 100 Hz
2.4
@Frequency 100 Hz
 2.4
@Frequency 1e+6 Hz
2.4
@Frequency 1e+6 Hz
Dielectric Strength 150 kV/mm3810 kV/in
Dissipation Factor  0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 165 µm/m-°C
@Temperature 20.0 °C
91.7 µin/in-°F
@Temperature 68.0 °F
Melting Point 133 °C271 °F
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °F
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C111 °F
Vicat Softening Point 75.0 °C167 °F
Flammability, UL94 HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
Oxygen Index 17 %17 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
LyondellBasell Lupolen 5231 HX HDPE, Impact Grade
Dow HDPE 10462N High Density Polyethylene
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Data

PSF069 / 66646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.