MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% glass fiber reinforced, PTFE lubricated polyamide 6.6 for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccDIN 53479
Water Absorption 0.80 %DIN 53495
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 175 MPaASTM-D638
Elongation at Break 3.0 %ASTM-D638
Tensile Modulus 8.30 GPaASTM-D790
Flexural Strength 250 MPaASTM D790
Flexural Modulus 6.80 GPaASTM-D790
Izod Impact, Notched 1.70 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmDIN 53482
 
Thermal PropertiesOriginal ValueComments
Melting Point 256 °C
Deflection Temperature at 0.46 MPa (66 psi) 243 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 227 °CDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram PlusTek PA840G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek PA360G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek PA865G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek PB300G6 Nylon 6, 30% Glass Fiber
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction

PPOLYRA241 / 57503

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.